ASA vapour smoothing is the quickest way to turn a ridged, matte FDM surface into a glossy part that looks almost injection-moulded: solvent vapour softens the outermost skin of the plastic in a controlled way, the layer lines flow together and the surface closes up. If you want to smooth ASA or chemically smooth ABS, acetone delivers excellent results – but when you try to smooth PETG, the process quickly hits chemical limits. In this guide we explain which materials are suitable, which parameters work, how to proceed step by step, which defects are typical and how to work safely.

What is vapour smoothing? Chemical smoothing instead of sanding

In vapour smoothing (also called chemical smoothing), a printed part is exposed to the vapour of a solvent that can dissolve exactly that plastic. The vapour condenses on the cooler surface and diffuses into the top polymer layer. There, the viscosity drops far enough for surface tension to pull the grooves between the layers smooth – much like a droplet flowing into a smooth dome. Once the solvent evaporates again, the surface solidifies as a closed, glossy skin.

The effect is limited to a thin outer zone of a few hundredths to a few tenths of a millimetre. Unlike sanding, it also reaches undercuts, inside corners and freeform surfaces evenly. At the same time, the process cannot tell layer lines from intended details: sharp edges, fine engravings and tight fits change as well. In return, the closed surface picks up less dirt and is more watertight.

Which materials can be chemically smoothed?

Whether chemical smoothing works depends on the combination of polymer and solvent:

ASA and ABS: the classic with acetone

ASA and ABS are amorphous styrene copolymers that dissolve readily in acetone. That is why ASA vapour smoothing with acetone is the best-documented and most reproducible process. ABS reacts slightly faster, ASA slightly slower and more evenly – both reach a high gloss. ASA also offers UV resistance, which makes smoothed ASA parts particularly popular for outdoor enclosures. An overview of the materials we print can be found on our 3D printing materials page.

Smoothing PETG: only to a limited extent

PETG is largely resistant to acetone. Ethyl acetate attacks PETG only weakly: in cold vapour it takes many hours, and the result is usually satin and uneven. Chlorinated solvents such as dichloromethane are effective – but they are harmful, suspected carcinogens and not an option for home users. To be honest: if you want to smooth PETG, sanding, filler and paint are the better choice. More on the material in our comparison PETG vs. PLA for functional parts.

PLA: why it practically does not work

PLA is a semi-crystalline polyester that barely dissolves in acetone. At best, acetone makes PLA dull or tacky. Solvents that actually attack PLA – such as dichloromethane, chloroform or tetrahydrofuran (THF) – are toxic or form explosive peroxides. Chemical smoothing is therefore not a sensible method for PLA.

Other combinations and fibre-reinforced filaments

PVB smooths well with isopropanol; HIPS reacts to limonene, which is used mainly to dissolve support structures. Fibre-reinforced grades such as ASA-CF or ABS-GF do become smoother, but the fibres remain at the surface – the result is matte rather than glossy (see fibre-reinforced 3D printing).

Parameter table: solvent, time and temperature by material

The following values are guide values for cold vapour at room temperature in a closed box. The actual time depends on box size, amount of solvent, temperature, part size and filament brand. Always start with a test part from the same spool.

MaterialSolventTime (cold vapour)TemperatureResultRisks
ABSAcetone20–60 minRoom temperatureHigh gloss, closed skinRounded edges, easy to overdo
ASAAcetone30–90 minRoom temperatureHigh gloss, even, UV-resistantBlushing in high humidity
ASA-CF / ABS-GFAcetone30–90 minRoom temperatureSmoother, but matteFibres remain visible
PETGEthyl acetateseveral hoursRoom temperatureSatin, often unevenWeak effect, stains
PETGDichloromethaneminuteslaboratory onlySmoothHealth hazard – not recommended
PLA– (acetone ineffective)––No usable resultEffective solvents are toxic
PVBIsopropanol15–60 minRoom temperatureGlossy, transparent with clear filamentFlammable vapours
Guide values for chemical smoothing in cold vapour (approx. 20–25 °C)

Times quoted in videos often refer to heated processes that take only minutes. Cold vapour takes longer, but is far easier to control.

Methods: cold vapour, hot vapour, cloth method and systems

Cold vapour in an acetone box

The standard method for ASA and ABS: a sealable glass or metal container is lined with paper towel moistened with a little acetone. At room temperature the vapour spreads evenly and the part smooths over 30 to 90 minutes. The method is forgiving and – following the safety rules – the only one we recommend outside professional environments.

Hot vapour: fast, but dangerous

Heating the solvent sharply increases the vapour concentration, and smoothing then takes only minutes. That is exactly what makes hot vapour risky: the concentration easily reaches the explosive range, and every heat source is a potential ignition source – especially hotplates with exposed contacts, thermostats or relays that spark when switching. Hot vapour belongs exclusively in closed systems designed for it.

Cloth method and brushing

Acetone is applied directly with a lint-free cloth or brush. This is fine for small touch-ups, but on whole parts it leaves wipe marks, drips and uneven gloss. Dipping in liquid acetone is even harder to control.

Professional systems

Industrial smoothing systems work with closed chambers, sometimes under vacuum, with metered solvent, controlled temperature and vapour recovery. For series parts with high demands on repeatability this is the right route; for one-offs an acetone box is usually sufficient.

ASA vapour smoothing step by step: smoothing ASA in an acetone box

You will need a glass or metal container with a lid, paper towel, a little acetone, a glass or metal spacer, butyl gloves and safety glasses.

  1. Prepare the part: Remove supports and brim, sand support remnants and burrs with 240 to 400 grit, wipe off dust. The solvent emphasises scratches rather than hiding them.
  2. Set up the workspace: Work outdoors or in a well-ventilated room, with no open flames, heaters or switching electrical devices nearby. Put on gloves and safety glasses.
  3. Prepare the chamber: Line the inner walls with paper towel and moisten it evenly with a little acetone, without puddles. Place the part on the spacer so that it touches neither paper nor liquid.
  4. Expose to vapour: Put the lid on and check the part through the glass every 10 to 15 minutes. ASA typically needs 30 to 90 minutes, ABS slightly less.
  5. Remove in time: As soon as the layer lines have flowed together and the surface is evenly glossy, lift the part out by the spacer. The surface is soft – do not touch it.
  6. Let it outgas: Leave the part for 24 to 48 hours in a well-ventilated place at room temperature until the surface is hard again.
  7. Check and rework: Check dimensions, ream holes, recut threads. If the result is still too matte, do a second short pass rather than extending the first.

Simply rest the lid on top – no significant pressure builds up at room temperature. Do not use containers made of polystyrene, ABS or other acetone-sensitive plastics.

Dimensional accuracy, strength and watertightness after smoothing

Dimensions and details

Chemical smoothing does not remove material, it redistributes it: the peaks of the layer lines flow into the valleys. External dimensions therefore usually stay within a few tenths of a millimetre, but edges round off visibly and small holes become slightly tighter. Text, knurling and fine features below about 0.4 mm lose sharpness. If you need tight fits, plan a tolerance allowance or rework functional surfaces after smoothing.

Strength and layer adhesion

The closed skin reduces the notch effect between layers; smoothed parts often feel slightly tougher and less prone to surface cracks. However, the process is not a strengthening measure: the interior remains unchanged, and parts exposed for too long lose stiffness as long as solvent is trapped inside. For functional parts, wall thickness, orientation and layer adhesion still matter most.

Watertightness

Small pores in the outer skin close up, so smoothed ASA and ABS parts are considerably more watertight than untreated prints. Larger defects, under-extrusion or gaps inside remain, however – containers and enclosures with sealing requirements should be tested under real conditions.

Defects and solutions in chemical smoothing

Most problems are caused by too much solvent, too long an exposure or unfavourable ambient conditions. The table helps with diagnosis:

DefectCauseSolution
Bubbles in the surfaceExposed for too long, damp filament or trapped solventShorten the time, dry the filament before printing, let the part outgas slowly at room temperature
White spots, milky hazeEvaporative cooling makes humidity condense; droplets on the surfaceWork in dry air, bring the part to room temperature, avoid drips from the lid
Rounded edges, lost detailsExposure too long, vapour too concentratedShorter exposure, less solvent, design details larger
Stress whitening and stress cracksSolvent meets residual stresses, press fits or heat-set insertsInstall inserts only after outgassing, smooth parts without load, print with low residual stress
Tacky, soft surfaceResidual solvent has not outgassedExtend outgassing to 48 hours, do not cover the part
Drip marks, uneven glossCondensate drips from the lid, paper too wet, uneven vapour distributionLess acetone, line the lid with paper too, place the part in the centre
Deformed thin wallsWalls too thin, solvent penetrates too deepAt least three perimeters, shorter exposure
Typical vapour smoothing defects and how to fix them

Safety: fire, explosion and health protection

Acetone, ethyl acetate and isopropanol are highly flammable. Acetone vapour is heavier than air, collects at floor level and forms an explosive mixture from about 2.5 per cent by volume – exactly the kind of concentration found in a smoothing box. Therefore:

  • No ignition sources: no open flames, cigarettes, fan heaters, soldering irons or hotplates with exposed contacts nearby. Light switches, relays and motors can also spark.
  • No heating: never heat solvents on hotplates, in a kettle, in an oven or in a microwave.
  • Ventilation: work outdoors or with windows open and cross-ventilation, not in a cellar or small, closed rooms.
  • Protective equipment: safety glasses and solvent-resistant gloves – butyl rubber gloves are suitable for acetone, nitrile only offers short-term splash protection. For longer work with vapours, use a half mask with an organic vapour filter; for acetone, filter type AX.
  • Small quantities: use only as much solvent as the paper can absorb, and close the stock container immediately.
  • Disposal: never pour residues down the drain. Collect soaked paper and solvent residues in a sealable metal container and take them to a hazardous waste collection point.

Dichloromethane, chloroform and THF do not belong in the workshop: they are harmful, some are suspected carcinogens, and dichloromethane is banned in paint strippers for consumers in the EU. Read the safety data sheet of the product before every use. Keep children and pets away from the workspace.

Slicer tips: preparing parts for chemical smoothing

Parts that will be chemically smoothed later are printed slightly differently from parts that stay raw:

  • More perimeters: At least three, preferably four perimeters (about 1.2 to 1.6 mm with a 0.4 mm nozzle). The solvent attacks the outermost wall, so there must be enough stable material behind it. Background in our guide to wall thickness and perimeters.
  • Moderate layer height: 0.15 to 0.2 mm is a good compromise. Finer layers shorten exposure time and preserve edges; very coarse layers take longer and round details more.
  • Tolerance allowance: Make holes and mating surfaces 0.1 to 0.2 mm larger. In PrusaSlicer use XY Size Compensation, in OrcaSlicer X-Y hole and contour compensation, in Cura Horizontal Expansion and Hole Horizontal Expansion.
  • Place the seam: The Z seam remains visible as a slight bump even after smoothing. Put it on a hidden side or on an edge; in OrcaSlicer the scarf seam can soften it further.
  • Iron top surfaces: For large, flat top surfaces, ironing in the slicer is good preparation – the surface is almost flat before smoothing.
  • No fuzzy skin, no supports on visible faces: Textures, embossed text below about 0.4 mm and support marks will not disappear during smoothing.

Alternatives: smoothing PETG without solvents, sanding, paint, epoxy

For PETG or PLA, tight tolerances or when solvents are not an option, these methods help:

  • Sanding: Step by step from 120 to 400 grit, then wet up to 800. Labour-intensive but dimensionally accurate – also the most practical way to smooth PETG.
  • Filler and paint: Spray filler or putty closes the layer lines; after intermediate sanding comes the top coat in any colour and gloss level.
  • Epoxy coating: Low-viscosity epoxy resin flows over the grooves and cures to a glossy finish – good for decorative parts, but it adds material.
  • Ironing and fine layers: Smooth top surfaces and less visible layer lines straight from the printer.

Our guide to 3D print surface finishing offers a detailed comparison of all methods from priming to painting. If you want to join smoothed parts into assemblies, choose an adhesive suited to ASA and ABS.

Have ASA and ABS parts printed for smooth surfaces

Do you need parts made of ASA, ABS, PETG or another engineering filament? Upload your model to our online calculator and get an instant price – material from 0.08 €/g plus from 3.90 € per print hour. We print in Berlin, including one-offs and small batches.

Frequently asked questions about vapour smoothing

Can PLA be smoothed with acetone?

No. PLA is largely resistant to acetone; at most the surface becomes dull or tacky. Solvents that do dissolve PLA are toxic or hard to control. For PLA, sanding, filler and paint are the better choice.

Can PETG be chemically smoothed?

Only to a limited extent. Acetone has hardly any effect on PETG, ethyl acetate works slowly and unevenly. Effective chlorinated solvents such as dichloromethane are harmful. If you want to smooth PETG, sanding and painting are the better option.

How long does ASA vapour smoothing take?

In cold acetone vapour at room temperature, typically 30 to 90 minutes. Afterwards the part should outgas for 24 to 48 hours before it is loaded, assembled or painted.

Is a smoothed part watertight?

The outer skin becomes much tighter because small pores close up. Larger defects and gaps between walls remain, however. Where sealing is required, design for watertightness and test the part.

Does vapour smoothing change the dimensions?

Yes, slightly: edges round off, small holes become tighter and fine details lose sharpness. Plan a tolerance allowance of 0.1 to 0.2 mm for fits or rework functional surfaces.

Is vapour smoothing dangerous at home?

Acetone is highly flammable and its vapours form explosive mixtures with air. Cold vapour, small quantities, good ventilation, no ignition sources and protective equipment greatly reduce the risk. Never heat solvents.

Can ASA-CF or ABS-GF be smoothed?

Partly. The matrix softens, but the fibres remain at the surface. The result is smooth and matte rather than high-gloss.

Can smoothed parts be glued or painted?

Yes, once fully outgassed. For paint, lightly key the surface so that the primer adheres. ABS and ASA can also be solvent-welded with acetone.


⚡ 3D Bäckerei Berlin
3D printing with 24h express from Berlin
Calculate price online ➔
📱 3D file on your PC?
Send yourself the direct link via Telegram or WhatsApp and upload your STEP/STL file comfortably on your computer: